The Effects of Heat Treatment with the ThermoWood (R) Method on the Equilibrium Moisture Content and Dimensional Stability of Wild Cherry Wood


Aytin A., Korkut S., Unsal O., Cakicier N.

BIORESOURCES, cilt.10, sa.2, ss.2083-2093, 2015 (SCI-Expanded) identifier identifier

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 10 Sayı: 2
  • Basım Tarihi: 2015
  • Doi Numarası: 10.15376/biores.10.2.2083-2093
  • Dergi Adı: BIORESOURCES
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus
  • Sayfa Sayıları: ss.2083-2093
  • İstanbul Üniversitesi Adresli: Evet

Özet

Low hygroscopicity is an important factor favoring the use of heat-treated wood materials. Hence, wild cherry (Cerasus avium (L.) Moench) wood was subjected to heat treatment with the ThermoWood (R) method for about 1 and 2 hours at temperatures of 190 and 212 degrees C in an industrial business. Then, trial samples were prepared and divided into two groups. By being conditioned in the environments of 20 degrees C and 65% relative humidity (WC1), 20 degrees C and 85% relative humidity (WC2), 20 degrees C and 30% relative humidity (WC3), and 23 degrees C and 50% relative humidity (WC4), equilibrium moisture content (EMC) and dimensional stability (DS) values of the samples in the first group were determined. The water thickness swelling (WTS) and water retention (WR) features of the samples of the second group were examined by keeping them in water both 24 and 72 h. The results show that EMC and WTS decreased with increasing treatment temperature and durations. Also, DS was improved. On the other hand, the WR values of all the samples stayed approximately the same.