THERMOCHIMICA ACTA, cilt.710, 2022 (SCI-Expanded)
Strontium cobaltite containing equimolar amounts of Sr and Co was produced by heating the mixture of SrCO3 and Co3O4 starting materials with a mole ratio of 1:0.333 under dynamic air atmosphere. The chemical reactions occurred during heating were determined and the intermediate and final products obtained at each critical temperature were characterized using TG/DTA-MS, ICP-OES, XRD and FT-IR analytical techniques. The volumetric analysis method (iodometric titration) and carbonation process were carried out to determine the oxygen stoichiometry of strontium cobaltite.