Chemical and Thermal Characterizations of Pinus sylvestris and Pinus pinaster
BIORESOURCES, cilt.15, sa.2, ss.3604-3620, 2020 (SCI-Expanded, Scopus)
- Yayın Türü: Makale / Tam Makale
- Cilt numarası: 15 Sayı: 2
- Basım Tarihi: 2020
- Doi Numarası: 10.15376/biores.15.2.3604-3620
- Dergi Adı: BIORESOURCES
- Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Academic Search Premier, CAB Abstracts, Chemical Abstracts Core, Compendex, Veterinary Science Database, Directory of Open Access Journals
- Sayfa Sayıları: ss.3604-3620
- İstanbul Üniversitesi Adresli: Hayır
Özet
Chemical and thermal aspects of Pinus sylvestris and Pinus pinaster were characterized, with consideration of non-extracted and cylohexaneethanol (EtOH)-extracted woods, holocellulose, and alpha-cellulose. The chemical properties including cylohexane-EtOH solubility of wood were determined by standard test methods, holocellulose, alpha-cellulose, lignin, and ash components. Fourier transform infrared attenuated total reflection spectroscopic (FTIR-ATR) analysis revealed changes in the chemical structure of the specimens. Lignin peaks were still observed in holocelluloses' spectra, and substantial loss of polysaccharides were also detected. Moreover, the alpha-cellulose spectra of both softwoods included bands belonging to polyoses. Pinus pinaster's holocellulose, alpha-cellulose, and ash contents were higher than those of Pinus sylvestris but lignin and cylohexane-EtOH-solubility amounts were lower. The mass loss during degradation stage of Pinus sylvestris and Pinus pinaster was observed in the extracted wood respectively as 73.0 and 74.5% within the 188.7 to 422.9 degrees C range. The highest mass loss for Pinus sylvestris and Pinus pinaster in the carbonization step was formed in their holocelluloses respectively as 22.9 and 22.5% from 426 degrees C to 1017 degrees C.